In the case of steel B, DCT generally has a positive trend, improving adhesive wear resistance by 10–65% (k = 0.1–1.6 × 10 −5 mm 3 /Nm).
← all excerpts
Effect of Deep Cryogenic Treatment on Wear and Galling Properties of High-Speed Steels.
2
—
—
The sentences
Steel B wear rate results are in range of 0.5–7.0 × 10 −7 mm 3 /Nm, with DCT generally resulting in a negative trend.