When the HA content increased from 0% to 25%, the degradation temperature for weight loss at 10% and 50% (T 10% and T 50% ) showed a trend of decreasing gradually, and both degradation temperature for weight loss at 80% and maximum value (T 80% and T max ) were increasing.
← all excerpts
Biodegradable 3D Printed Scaffolds of Modified Poly (Trimethylene Carbonate) Composite Materials with Poly (L-Lactic Acid) and Hydroxyapatite for Bone Regeneration.