Neither PDeF nor rGO significantly affects the bands at 869 and 755 cm −1 , relative to PLA’s amorphous and crystalline regions, respectively, as neither the position nor the intensity of these bands shows a clear trend with the sample composition.
← all excerpts
Improving the Thermomechanical Properties of Poly(lactic acid) via Reduced Graphene Oxide and Bioderived Poly(decamethylene 2,5-furandicarboxylate).