However, at 7, 14, and 28 days, all the mortars with 7% of coarse silica fume followed a clear trend, i.e., the higher the limestone content, the lower the flexural strength.
← all excerpts
Mechanical Performance of Portland Cement, Coarse Silica Fume, and Limestone (PC-SF-LS) Ternary Portland Cements.