31 The elongation at the break of the composite membrane showed a trend of fall-rise, when the TM NPs content was 2 wt%, the elongation at break of the composite film was the lowest (72.65 ± 6.85%), which could not meet the requirement for the coronary artery (99%). 32 The composite membrane containing 6 wt% or 8 wt% of TM NPs had good toughness with an elongation at break of more than 100%.