Their thermal conductivities were measured at different temperatures allowing observation of a clear trend relating the initial formulation with the porous structure and reaching values as low as 12 mW/mK, the lowest found in the literature for aerogels based on this polymer matrix.
← all excerpts
Super-Insulating Transparent Polyisocyanurate-Polyurethane Aerogels: Analysis of Thermal Conductivity and Mechanical Properties.