Barely Significant
← all excerpts

Meso-Scale Observations of the Evolution of Matrix/Filler Interface Dewetting During NEPE Propellant Aging.

Polymers (Basel) · 2026 · PMC13259173 · PMID 42280537

2
hedged sentences
closest p
boldest claim

The sentences

showed a trendno p-value reported
As shown in Figure 8 , under 20% fixed strain, the porosity within the matrix showed a trend of declining with an increase in aging time.

also in 53,322 other papers

a clear trendno p-value reported
Compared to the specimen aged for 9 weeks, the specimen aged for 12 weeks exhibited more pronounced matrix softening, showing a clear trend towards a paste-like consistency.